Anycubic Kobra 3 V2 + ACE Pro โ€” Material Settings Reference

Aug 8, 2026 11:25am · 168 views
kobra3d printingfdmmaterialssettingsplapetgtpuabscura1c3d
Markdown

Anycubic Kobra 3 V2 + ACE Pro โ€” Material Settings Reference

Multi-color FDM. CoreXY. ACE Pro 4-filament hub. Main workhorse for functional parts, multi-color prints, and prototypes.

Hardware Specs

  • Build volume: 250 ร— 250 ร— 260 mm
  • Motion: CoreXY | Extruder: Direct drive, dual-gear
  • Nozzle: 0.4 mm hardened steel (stock) | Max temp: 300ยฐC
  • Bed: PEI spring steel, magnetic | Max temp: 110ยฐC
  • Slicer: Orca Slicer (recommended) or Anycubic Slicer
  • Firmware: Klipper-based

---

PLA (Standard)

SettingValue
Nozzle temp215โ€“220ยฐC
Bed temp60ยฐC
First layer bed65ยฐC
Print speed150โ€“200 mm/s
First layer speed30 mm/s
Cooling fan100% after layer 2
Retraction0.8 mm @ 35 mm/s
Layer height0.2 mm (0.1โ€“0.28 mm range)
EnclosureOpen

Notes: Most forgiving material. Stringing on multicolor: increase retraction to 1.0โ€“1.2 mm. PLA+ runs 5ยฐC hotter. Matte PLA needs 225ยฐC and slightly slower speeds.

---

PLA+ / PLA Pro

SettingValue
Nozzle temp220โ€“230ยฐC
Bed temp65ยฐC
Print speed120โ€“180 mm/s
Cooling fan100%
Retraction1.0 mm @ 35 mm/s

Notes: Better layer adhesion and impact resistance than standard PLA. Slightly more prone to stringing. Good for brackets, enclosures, snap fits.

---

PETG

SettingValue
Nozzle temp235โ€“245ยฐC
Bed temp80โ€“85ยฐC
First layer bed90ยฐC
Print speed80โ€“120 mm/s
First layer speed25 mm/s
Cooling fan40โ€“60%
Retraction1.2โ€“1.5 mm @ 30 mm/s
Layer height0.2โ€“0.25 mm
EnclosureOpen

Notes: Hygroscopic โ€” dry before printing (65ยฐC, 6 hrs). Sticks hard to PEI โ€” use glue stick or lower bed to 75ยฐC if removing parts is difficult. Great for mechanical parts, brackets, outdoor use. Stringing is common; keep retraction high and travel speed fast (200 mm/s).

---

TPU (Flexible, Shore 95A)

SettingValue
Nozzle temp225โ€“235ยฐC
Bed temp40โ€“50ยฐC
Print speed25โ€“40 mm/s
First layer speed20 mm/s
Cooling fan30โ€“50%
Retraction0โ€“1.0 mm (minimal)
Layer height0.2 mm
EnclosureOpen

Notes: Direct drive handles TPU well. Print slow โ€” 35 mm/s max or you'll get clogs. Disable or minimize retraction to avoid grinding. No ACE Pro for TPU โ€” load single-filament direct. Shore 85A = even slower (20 mm/s). Dry at 50ยฐC 4 hrs if moisture issues.

---

ABS

SettingValue
Nozzle temp240โ€“250ยฐC
Bed temp100โ€“110ยฐC
First layer bed110ยฐC
Print speed60โ€“80 mm/s
Cooling fan0โ€“20% (very low)
Retraction1.0 mm @ 30 mm/s
Layer height0.2 mm
EnclosureRequired โ€” improvise with cardboard if needed

Notes: Warps badly without enclosure. Brim of 8โ€“10 mm required on anything over 50 mm. Fumes โ€” print in ventilated area or outside. ABS-acetone slurry on bed helps adhesion. Excellent for parts that need post-processing (acetone smoothing), heat resistance up to 100ยฐC.

---

ASA

SettingValue
Nozzle temp245โ€“255ยฐC
Bed temp100โ€“110ยฐC
Print speed60โ€“80 mm/s
Cooling fan0โ€“10%
Retraction1.0 mm @ 30 mm/s
EnclosureRequired

Notes: UV-stable ABS alternative. Use for anything outdoors. Same printing pain as ABS but worth it. Slightly less warp-prone than ABS. Good for car parts, outdoor mounts, enclosure handles.

---

PLA-CF / PETG-CF (Carbon Fiber Filled)

SettingValue
Nozzle temp (PLA-CF)220โ€“230ยฐC
Nozzle temp (PETG-CF)240โ€“250ยฐC
Bed temp65ยฐC (PLA) / 85ยฐC (PETG)
Print speed60โ€“100 mm/s
Cooling fan80โ€“100% (PLA-CF) / 30% (PETG-CF)
Nozzle requiredHardened steel 0.4 mm minimum

Notes: Abrasive โ€” destroys brass nozzles fast. Already on hardened steel. Stiffer, lighter than base material. Good surface finish. Higher strength-to-weight. Use for tooling, jigs, brackets.

---

PA/Nylon

SettingValue
Nozzle temp250โ€“270ยฐC
Bed temp70โ€“90ยฐC
Print speed40โ€“60 mm/s
Cooling fan20โ€“40%
Retraction1.5 mm @ 30 mm/s
EnclosureStrongly recommended
Drying requiredYes โ€” 80ยฐC, 12 hrs minimum

Notes: Extremely hygroscopic. Print same day as drying. Excellent impact/abrasion resistance. Bed adhesion is tricky โ€” PEI with glue stick or Garolite sheet. PA12 is easier than PA6. Good for gears, hinges, functional wear parts.

---

PVA (Support Soluble)

SettingValue
Nozzle temp185โ€“200ยฐC
Bed temp60ยฐC
Print speed30โ€“40 mm/s
Cooling fan50โ€“80%
Retraction1.2 mm @ 25 mm/s

Notes: ACE Pro use โ€” PVA in one channel, main material in another. Dissolves in water (warm water speeds it up). Keep bone dry โ€” absorbs moisture within hours of opening. Print PVA slower and cooler than PLA. Compatible with PLA supports. Store with desiccant sealed.

---

Multi-Color / ACE Pro Tips

  • Color change purge: 80โ€“120 mmยณ purge block minimum per color swap. More for lightโ†’dark transitions.
  • Purge into support: Enable in Orca Slicer to avoid large purge towers.
  • Tension: Keep filament paths short and straight to the ACE Pro hub.
  • Humidity: The hub has no dryer โ€” pre-dry hygroscopic materials.
  • Speed during swap: ACE Pro slows print during color change โ€” normal.
  • Max colors: 4 via hub, can extend to 8+ with manual swaps.

---

Calibration / Tuning

  • First layer: Z-offset critical โ€” live adjust first layer to slight squish
  • PA (Pressure Advance): 0.02โ€“0.06 for PLA, 0.04โ€“0.08 for PETG, 0.0 for TPU
  • Flow rate: Calibrate per filament spool โ€” 0.95โ€“1.05 typical range
  • Retraction tune: Print retraction tower per material
  • Temp tower: Run for new brands โ€” find sweet spot for each

---

Common Issues

ProblemFix
StringingIncrease retraction, raise travel speed, lower temp 5ยฐC
Layer separationRaise temp 5ยฐC, slow down, check filament diameter
Bed not stickingClean PEI with IPA, check Z offset, raise first layer temp
CloggingCheck temp, slow speed, dry filament, check nozzle
WarpingHigher bed temp, brim, enclosure, draft shield
Blobs/zitsTune coasting and retraction