Stringing and hairy prints
Thin wisps of plastic between parts of the print, like cobwebs.
Fine hairs between towers or across gaps, sometimes small blobs where the nozzle starts moving again.
Causes and fixes, most likely first
Wet filament
Damp filament boils in the nozzle and oozes. PETG, TPU and nylon soak up water within days; even PLA gets bad over weeks. Popping or crackling sounds while printing are a giveaway.
Nozzle too hot
Hotter plastic is runnier and oozes during travel moves.
Retraction not tuned
Retraction pulls the filament back before a travel move. Too little leaves strings; too much on a Bowden setup can cause gaps and clogs.
Slow or long travel moves
The longer the nozzle hangs over open air, the more it drips.
Commands and settings by firmware
Set retract_length and retract_speed in [firmware_retraction] if you use firmware retraction, or tune it in the slicer. Tune pressure advance first: it reduces oozing at the ends of lines.
Slicer retraction is normal. Tune Linear Advance (M900 K) first if your firmware has it enabled.
Run Flow Dynamics calibration for each filament in Bambu Studio, and dry the spool. Bambu's default retraction is already tuned for the hotend.
Guides that go deeper
- 3D Printing Troubleshooting Guide: Fix Layer Shifts, Stringing, Warping, and 30+ Common Problems
- Direct Drive vs Bowden Extruders: Trade-offs, Retraction Tuning, and Conversion
- 3D Print Troubleshooting: Stringing, Warping, Layer Splitting, and Elephant Foot
- Ironing Settings in FDM Slicers: When It Helps, When It Causes Pinholes and Stringing
Other 3d printer problems
Still stuck?
Post a photo of the print and your settings in the forum, or get live help from someone online now.