← Materials
PLA

Elegoo Neptune 4 — PLA Matte

⚙ Elegoo Neptune 4 Tested 2025
4/5
Notes
Matte PLA uses the same profile as standard PLA. Run 5°C hotter than your PLA baseline for better layer adhesion. Most matte brands have matte additive that slightly affects flow.
Tips
Calibrate flow rate — matte PLA often under-extrudes at standard PLA settings. Try 100-102% flow.
Details

Matte PLA uses the same profile as standard PLA. Run 5°C hotter than your PLA baseline for better layer adhesion. Most matte brands have matte additive that slightly affects flow.

Temperatures

SettingValue
Nozzle225 °C
Bed60 °C
First Layer Bed65 °C

Speed

SettingValue
Print Speed200 mm/s
First Layer Speed40 mm/s

Cooling

SettingValue
Fan Speed100 %

Retraction

SettingValue
Distance0.8 mm

Quality

SettingValue
Layer Height0.2 mm
Flow Rate101 %

Tips