Notes
Matte PLA uses the same profile as standard PLA. Run 5°C hotter than your PLA baseline for better layer adhesion. Most matte brands have matte additive that slightly affects flow.
Tips
Calibrate flow rate — matte PLA often under-extrudes at standard PLA settings. Try 100-102% flow.
Details
Matte PLA uses the same profile as standard PLA. Run 5°C hotter than your PLA baseline for better layer adhesion. Most matte brands have matte additive that slightly affects flow.
Temperatures
| Setting | Value |
|---|---|
| Nozzle | 225 °C |
| Bed | 60 °C |
| First Layer Bed | 65 °C |
Speed
| Setting | Value |
|---|---|
| Print Speed | 300 mm/s |
| First Layer Speed | 60 mm/s |
Cooling
| Setting | Value |
|---|---|
| Fan Speed | 100 % |
Retraction
| Setting | Value |
|---|---|
| Distance | 0.6 mm |
Quality
| Setting | Value |
|---|---|
| Layer Height | 0.2 mm |
| Flow Rate | 101 % |
Tips
Calibrate flow rate — matte PLA often under-extrudes at standard PLA settings. Try 100-102% flow.