Notes
Wood fill PLA contains real wood particles. Prints close to standard PLA but slower and hotter. The matte surface mimics wood grain and can be sanded and stained.
Tips
Go slow for best layer adhesion and wood texture. Avoid over-cooling — reduce fan 30-50%. Sanding with 220 grit after printing gives authentic wood feel. Use hardened nozzle.
Details
Wood fill PLA contains real wood particles. Prints close to standard PLA but slower and hotter. The matte surface mimics wood grain and can be sanded and stained.
Temperatures
| Setting | Value |
|---|---|
| Nozzle | 230 °C |
| Bed | 60 °C |
| First Layer Bed | 65 °C |
Speed
| Setting | Value |
|---|---|
| Print Speed | 100 mm/s |
| First Layer Speed | 40 mm/s |
Cooling
| Setting | Value |
|---|---|
| Fan Speed | 30 % |
Retraction
| Setting | Value |
|---|---|
| Distance | 0.8 mm |
Quality
| Setting | Value |
|---|---|
| Layer Height | 0.25 mm |
| Flow Rate | 100 % |
Notes
| Setting | Value |
|---|---|
| Nozzle Type | Hardened steel recommended important |
| Post Process | Sand with 220 grit, stain with wood stain for authentic look |
Tips
Go slow for best layer adhesion and wood texture. Avoid over-cooling — reduce fan 30-50%. Sanding with 220 grit after printing gives authentic wood feel. Use hardened nozzle.