Notes
PA6 (Nylon 6) is tougher but harder to print than PA12. Higher temp, more warping, more moisture sensitivity. Reward is exceptional toughness.
Tips
PA6 absorbs moisture faster than almost any other filament. Never print day-old open PA6. Brim is essential. Slow down 50% vs PA12.
Details
PA6 (Nylon 6) is tougher but harder to print than PA12. Higher temp, more warping, more moisture sensitivity. Reward is exceptional toughness.
Temperatures
| Setting | Value |
|---|---|
| Nozzle | 285 °C |
| Bed | 100 °C |
| First Layer Bed | 105 °C |
Speed
| Setting | Value |
|---|---|
| Print Speed | 48 mm/s |
| First Layer Speed | 15 mm/s |
Cooling
| Setting | Value |
|---|---|
| Fan Speed | 0 % |
Retraction
| Setting | Value |
|---|---|
| Distance | 0.5 mm |
Quality
| Setting | Value |
|---|---|
| Layer Height | 0.15 mm |
Notes
| Setting | Value |
|---|---|
| Drying | Dry 16h @ 80°C — never print open PA6 critical |
| Adhesion | Large brim required important |
Tips
PA6 absorbs moisture faster than almost any other filament. Never print day-old open PA6. Brim is essential. Slow down 50% vs PA12.