Notes
TPU works in the P1S but AMS is not recommended — run direct from spool.
Tips
Bypass AMS for TPU. Run single spool directly into extruder. Disable retraction.
Details
TPU works in the P1S but AMS is not recommended — run direct from spool.
Temperatures
| Setting | Value |
|---|---|
| Nozzle | 230 °C |
| Bed | 35 °C |
Speed
| Setting | Value |
|---|---|
| Print Speed | 40 mm/s |
| First Layer Speed | 20 mm/s |
Cooling
| Setting | Value |
|---|---|
| Fan Speed | 0 % |
Retraction
| Setting | Value |
|---|---|
| Distance | 0 mm (disabled) |
Quality
| Setting | Value |
|---|---|
| Layer Height | 0.2 mm |
Tips
Bypass AMS for TPU. Run single spool directly into extruder. Disable retraction.